Back to blog
Article

Causes of Cracks in Cement Prefabricated Houses

Admin September 18, 2026

The essence of cracks in cement prefabricated houses is the result of the interaction between materials and the environment, primarily stemming from four major factors: temperature stress, material shrinkage, foundation settlement, and production process defects.

  1. Temperature Stress
    The coefficient of thermal expansion of concrete is 1×10⁻⁵/℃. When the ambient temperature difference exceeds 20℃, the walls may develop fine cracks of 0.1-0.2mm due to thermal expansion and contraction. For example, in northern regions during winter, when the day-night temperature difference reaches 15℃, walls on the sunny side and shaded side are prone to cracking due to uneven temperatures. Such cracks are mostly horizontally distributed, consistent with the direction of the temperature gradient.

  2. Material Shrinkage
    During the hardening process of concrete, water evaporation causes shrinkage deformation, with a shrinkage rate of approximately 0.02%-0.04%. If the cement content is too high (>400kg/m³) or curing is insufficient, shrinkage cracks may increase to 0.25mm. Additionally, high-grade cement is prone to cracking due to concentrated hydration heat; excessive mud content in sand can lead to spiderweb-like cracks after concrete drying shrinkage; uncontrolled water-cement ratio (such as when construction teams add water arbitrarily) significantly reduces concrete strength, causing the floor slab to become loose even before use.

  3. Foundation Settlement
    When the differential settlement of the foundation exceeds 30mm, the walls are subjected to shear stress, potentially resulting in diagonal cracks wider than 0.3mm. Such cracks often appear at the corners of the house or around door and window openings, consistent with the direction of foundation deformation, and can lead to structural instability in severe cases.

  4. Production Process Defects

    • Inadequate mold vibration compaction: When the air bubble content exceeds 5%, micro-cracks of less than 0.1mm may appear on the surface of prefabricated components.
    • Excessive temperature difference during steam curing: If the heating or cooling rate exceeds 20℃/h, inconsistent shrinkage between the interior and exterior of the component can lead to surface cracking.
    • Excessive mixing and transportation time: Prolonged mixing or transportation causes water evaporation in the concrete, reducing slump and leading to irregular shrinkage cracks after hardening.
    • Non-standard vibration operations: Insufficient vibration results in honeycombing and pitting inside the concrete, while excessive vibration causes aggregate separation. The upper layer of fine aggregates has greater drying shrinkage, forming plastic shrinkage cracks.
    • Arbitrary changes to the mix ratio: Unauthorized increases in water content or water-cement ratio significantly increase hardening shrinkage, resulting in net-like or irregular cracks of varying lengths.
    • Disorganized construction management: Improper stacking of machinery and materials may cause secondary damage to completed parts, increasing the risk of cracks.