I. Wood Selection Criteria
- Species Selection: For load-bearing structural systems, priority is given to coniferous woods such as Douglas fir, Scots pine, SPF (Spruce-Pine-Fir), and Southern pine. Their design values for flexural strength must be ≥15 MPa, and the modulus of elasticity ≥10,000 MPa.
- Grading Selection: Implement graded management based on the functional differences of components. Key load-bearing components like roof trusses and main beams use Grade Ia wood, requiring a grain slope ≤1/20 and a single live knot diameter ≤1/5 of the cross-section width. Secondary load-bearing components such as secondary beams and wall studs use Grade II wood, allowing a small number of dead knots with diameters ≤30mm. Decorative components like eaves boards and window frames use premium-grade wood, ensuring a knot-free surface and uniform color.
- Testing Requirements: All wood must be accompanied by a mechanical performance report issued by a provincial-level or higher testing institution. Upon arrival, randomly sample 3 groups from each batch of 200m³ for flexural strength re-testing to ensure material performance meets design standards.
II. Moisture Content Control
- Drying Process: Adopt a two-stage drying method of kiln drying followed by natural balancing. The first stage involves drying in a 105℃ kiln environment to a moisture content of 20%, with the heating rate controlled at 5℃/h to prevent surface cracking. The second stage involves natural balancing in a ventilated shed for 15 days to achieve a moisture content gradient ≤3%.
- Moisture Content Standards: The final moisture content of load-bearing components must be controlled within the 12%-18% range, while horizontal components like floor and roof panels must have a moisture content ≤15%. Testing is conducted using a resistance-type moisture meter, with samples taken at 200mm from the end and at the center. The acceptance criterion is a difference ≤2% among the three samples.
III. Protective Treatment
- Preservative Treatment: Components in contact with the foundation, such as ground beams and wooden columns, are treated with ACQ-D type preservative using vacuum-pressure impregnation. Maintain a vacuum of -0.09 MPa for 30 minutes, then pressurize to 1.2 MPa for 2 hours to ensure a preservative penetration depth ≥25mm and a drug loading of 6kg/m³. After treatment, allow natural curing for 7 days until the surface moisture content drops below 20% before installation.
- Fire Protection Treatment: Load-bearing components are coated with ultra-thin intumescent fire-retardant coating (dry film thickness of 3.5mm), applied in three layers using airless spraying technology, with an 8-hour interval between each layer. After the coating dries, conduct fire resistance testing, requiring that under a 600℃ open flame, the time for the backfire surface temperature to rise to 220℃ is ≥90 minutes. Weak areas like wooden truss joints require additional wrapping with fiberglass cloth to enhance fire resistance.
- Insect Protection Treatment: After degreasing, the wood is sprayed with a permethrin-based insect repellent (concentration of 0.5%), focusing on mortise-and-tenon joints, component ends, and cracks. Areas prone to insect infestation, such as eaves and floor joists, require the installation of insecticide diffusion holes with a diameter of 10mm, spaced 300mm apart in a quincunx pattern.