The construction of prefabricated house lintel steel bars should be standardized in terms of steel bar selection, dimensions, installation, concrete, and curing. The specific key points are as follows:

Steel Bar Selection: The main reinforcement must use HRB400-grade steel bars, with commonly used diameters ranging from φ10 to φ16. For the main reinforcement of prefabricated door lintels, the diameter requirements are φ10 or φ12. Stirrups should be selected from HPB300-grade steel bars with a diameter of 8mm, and the spacing between stirrups should not exceed 200mm to ensure the shear-bearing capacity of the lintel.

Dimension Requirements: The width of the lintel should be consistent with the thickness of the brick wall. For example, a 24-wall should be made 24 centimeters wide. The support length extending into the wall on both ends should meet the specifications: for ordinary houses, the support length on each side should not be less than 240mm (i.e., 25 centimeters), while in earthquake-prone areas, it should be extended to 300mm (i.e., 30 centimeters) to enhance structural stability.

Installation Key Points: During installation, the main reinforcement must face downward to ensure the correct direction of force application; the length extending into the wall on each side should not be less than 240mm to avoid cracking due to insufficient support. When fabricating the lintel, its width should be appropriately reduced (e.g., by 5-10mm) to accommodate the installation gap in the wall; during steel bar binding, the position of the main reinforcement should be accurately located to prevent displacement that could affect structural performance.

Concrete Requirements: The concrete grade should not be lower than C20. If the lintel is in a humid environment (such as basements or bathrooms), the grade should be increased to C25 to enhance impermeability and durability. Concrete pouring should be vibrated and compacted to avoid defects such as honeycombing and pitting.

Curing Requirements: After pouring, curing should be carried out. In ordinary environments, the curing period should not be less than 7 days; if the lintel has waterproofing requirements or is in special environments (such as low temperatures or dry conditions), the curing time should be extended to 14 days to ensure full development of concrete strength.

Precautions: Before construction, the design drawings should be checked to confirm the lintel dimensions, steel bar specifications, and support lengths; during steel bar processing, bending damage should be avoided, and stirrup ends should be bent at a 135° angle; during installation, if the wall is made of hollow bricks or aerated blocks, concrete pads should be poured at the support points to prevent local crushing.