Treatment Methods for Gaps in Prefabricated Houses
Quản trị 18 tháng 9, 2026
The treatment methods for gaps in prefabricated houses should be selected based on the type and severity of the gaps, and can be specifically divided into three categories: ordinary panel gap treatment, crack repair, and reinforcement with special materials.

I. Ordinary Panel Gap Treatment (During Installation)
- Adjusting Panel Gap Width: During installation, control the gap difference through reasonable panel arrangement to ensure that the gap width is ≤30mm, avoiding structural issues caused by excessive gap differences in the later stage.
- Filling with Fine Aggregate Concrete: When the gap difference is 20-40mm, use fine aggregate concrete with a strength grade of C20 or above for filling. If necessary, add steel bars or wire mesh to the concrete to enhance its crack resistance.
- Reinforcing with Cast-in-Place Concrete Strip: If the gap difference is ≥50mm, it is necessary to add a cast-in-place concrete strip with a width of not less than 200mm at the panel gap, and configure longitudinal steel bars inside to form an integral load-bearing structure.
- Reinforcing with Additional Steel Bars: For through cracks or areas with large gap differences, add Φ6-Φ8 steel bars at the bottom or top of the panel gap to enhance structural stability.
II. Crack Repair (For Existing Houses)
- Minor Crack Treatment: If there are few cracks, small gaps, and no liquid leakage, repair can be temporarily postponed, but regular observation of crack changes is required.
- Repair Process for Larger Cracks:
- Chiseling the Gap: Chisel away 5cm of the surface layer on both sides of the crack to make the joint surface slope-shaped and roughened, increasing the bonding area.
- Base Layer Cleaning: Thoroughly remove dust and loose particles to ensure tight bonding between the repair material and the base layer.
- Brushing with Cement Mortar: Brush pure cement mortar (water-cement ratio of 0.4-0.5) inside the panel gap to seal the gap and enhance bonding strength.
- Pouring Concrete in Stages: Pour the concrete to half the depth of the panel gap for the first time, and then pour it to 1cm from the panel surface for the second time after absorption, compacting and leveling to avoid voids.
- Curing Requirements: After repair, cure for at least 2-3 days, and strictly prohibit treading during this period to prevent damage to the unsolidified material.
III. Reinforcement with Special Materials (For Shrinkage Cracks or Structural Reinforcement)
- Non-shrinkage Epoxy Structural Assembly Adhesive: Using this type of adhesive when assembling prefabricated panels can reduce the risk of cracks caused by material shrinkage in the later stage.
- Carbon Fiber Cloth Reinforcement Process:
- Chiseling the Gap and Leveling: Chisel the crack into an inverted V-shape, clean the dust, and level the base layer with repair adhesive.
- Brushing with Impregnating Adhesive: Brush carbon fiber impregnating adhesive on the crack surface, paste carbon fiber cloth, and scrape out air bubbles to ensure compactness.
- Secondary Application of Adhesive: Apply modified epoxy impregnating adhesive on the surface of the carbon fiber cloth again to form a protective layer.
- Filling with Epoxy Repair Adhesive: For opened cracks, chisel out the inverted V-shape and fill with non-shrinkage epoxy repair adhesive, then polish it flat and paste carbon fiber cloth to enhance tensile strength.
Precautions: Avoid drilling holes in the prefabricated panels when treating cracks to prevent damage to the load-bearing structure; when installing hanging rods for ceiling construction, they should be installed in the gaps between two prefabricated panels; when using mortar or epoxy mortar for repair, pay attention to the shrinkage of the material to avoid secondary cracking.