Quay lại blog
Bài viết

What is the Gap Size in Prefabricated Houses

Quản trị 18 tháng 9, 2026

The gap size in prefabricated houses needs to be discussed on a case-by-case basis, as the standards vary depending on the location and purpose of the gaps.

Gap between two prefabricated panels during installation: During the installation of prefabricated panels, a gap of 20~40mm should be left between two panels. This gap is set to accommodate minor deformations that may occur during the installation and use of the prefabricated panels, preventing mutual extrusion between the panels due to factors such as temperature changes and load effects, which could lead to cracks or other structural issues. Meanwhile, an appropriate gap also provides operating space for subsequent gap treatment.

Length requirements for placing prefabricated panels on concrete members or walls: When a prefabricated panel is placed on a concrete member (such as a ring beam), its placement length should not be less than 80mm; when placed on a wall, the placement length should not be less than 100mm. This requirement ensures that there is sufficient contact area between the prefabricated panel and the supporting structure, thereby guaranteeing structural stability and safety. If the placement length is insufficient, it may cause the prefabricated panel to slip or overturn under load, posing a threat to the overall structure of the house.

Gap treatment between prefabricated panels: After the installation of prefabricated panels is completed, the panel gaps need to be treated. First, the debris inside the gaps should be cleaned up to ensure that there are no dust, fragments, or other impurities inside the gaps. Then, cement mortar should be used for pouring and vibrated densely to ensure the density and strength of the gap filling. If the gap is large, concrete should be used for on-site pouring and solidification, and curing should be carried out. It is prohibited to fill the gaps with bricks, as the strength and durability of bricks differ from those of concrete, and filling gaps with bricks may affect the overall performance of the structure.

Danger standards for cracks in the roof of prefabricated panel houses: According to the 'Technical Guidelines for Structural Safety Inspection of Self-built Houses', cracks in prefabricated panels exceeding 1 millimeter require vigilance. If they are load-bearing cracks, such as horizontal cracks that appear when the roof sags, attention should be paid even if they are only 0.8 millimeters. The location of the cracks is also crucial. If the cracks extend from the roof to two-thirds of the wall height or are exactly on the load-bearing beam, the danger coefficient doubles; if the cracks continue to lengthen and widen, even if they have not reached 1 millimeter, a professional organization should be consulted for inspection.