The emergence of cracks in the walls of prefabricated houses is essentially the result of the interaction between materials and the environment, primarily stemming from factors such as temperature stress, material shrinkage, foundation settlement, production processes, and splicing issues.

  1. Temperature Stress: The coefficient of thermal expansion for concrete is 1×10⁻⁵/℃. When the environmental temperature difference exceeds 20℃, the walls may develop fine cracks ranging from 0.1 to 0.2mm due to thermal expansion and contraction. For example, in northern winters, when the day-night temperature difference reaches 15℃, the walls on the sunny and shady sides are prone to cracking due to uneven temperatures.
  2. Material Shrinkage: During the hardening process of concrete, water evaporation causes shrinkage deformation, with a shrinkage rate of approximately 0.02% to 0.04%. If the cement content is too high (>400kg/m³) or curing is insufficient, shrinkage cracks may increase to 0.25mm.
  3. Foundation Settlement: When the differential settlement of the foundation exceeds 30mm, the walls will be subjected to shear stress, potentially resulting in diagonal cracks with widths exceeding 0.3mm. During ground settlement, different parts descend at varying speeds, such as uneven settlement on the left and right sides of a building, which can easily lead to wall cracking.
  4. Production Process: If the mold is not vibrated densely (air bubble rate >5%) or the temperature difference during steam curing is too large (>20℃/h), surface cracks less than 0.1mm may occur during the prefabrication stage.
  5. Splicing Issues: Prefabricated panel houses are constructed by splicing individual prefabricated panels together, with the splicing points being inherently weak areas of the walls. Thermal expansion and contraction, combined with inadequate reinforcement or failure to reserve reasonable expansion joints during installation of the two panels, can also lead to cracks.

According to the 'Code for Acceptance of Constructional Quality of Concrete Structures' (GB50204-2015), crack control for prefabricated components is divided into three levels. In ordinary residential environments, walls of cement houses are allowed to have cracks with widths ≤0.25mm. These cracks are considered 'harmless cracks' that only affect aesthetics and do not require structural reinforcement. When the crack width exceeds 0.3mm or is through-going (penetrating the wall), it is necessary to check whether they are caused by foundation settlement or excessive structural loads, requiring intervention from a professional team for repair.