Cracking in prefabricated concrete houses can be caused by various factors such as temperature stress, material shrinkage, foundation settlement, and production processes, and the need for repair should be determined based on the width and nature of the cracks.

I. Causes of Cracking

  1. Temperature Stress: The coefficient of thermal expansion of concrete is 1×10⁻⁵/℃. When the ambient temperature difference exceeds 20℃, the walls may develop fine cracks ranging from 0.1 to 0.2mm due to thermal expansion and contraction. For example, in northern regions during winter, when the day-night temperature difference reaches 15℃, the walls on the sunny side and the shady side are prone to cracking due to uneven temperature distribution.
  2. Material Shrinkage: During the hardening process of concrete, water evaporation causes shrinkage deformation, with a shrinkage rate of approximately 0.02% - 0.04%. If the cement content is too high (>400kg/m³) or curing is insufficient, shrinkage cracks may increase to 0.25mm.
  3. Foundation Settlement: When the differential settlement of the foundation exceeds 30mm, the walls will be subjected to shear stress, potentially resulting in diagonal cracks with widths exceeding 0.3mm.
  4. Production Process: Inadequate vibration compaction of the mold (air bubble content >5%) or excessive temperature differences during steam curing (>20℃/h) may lead to surface cracks of less than 0.1mm during the prefabrication stage.

II. Crack Classification and Treatment

According to the "Code for Acceptance of Constructional Quality of Concrete Structures" (GB50204 - 2015), crack control in prefabricated components is classified into three levels:

  • Ordinary Residential Environment: Cracks with widths ≤0.25mm are allowed in the walls of concrete houses. These cracks are considered "harmless" and only affect aesthetics, requiring no structural reinforcement.
  • Repair Required: When the crack width exceeds 0.3mm or is through-wall (penetrating the wall), it is necessary to determine whether it is caused by foundation settlement or excessive structural loads, and professional teams should be involved in the repair.

III. Practical Case Warnings

An elderly couple in Lingwu, Ningxia, purchased a prefabricated concrete mobile home that developed extensive cracking due to quality issues, rendering it uninhabitable. In another case, a real estate project used 3D prefabricated floor slabs, which cracked on the roof due to non-compliant construction. After removal, it was found that there was "extensive honeycombing in the concrete and exposed and severely rusted steel bars." These cases indicate that material quality, construction compliance, and acceptance inspection are key to preventing cracking.